适用范围 电子装配车间、服装车间、手术室等轻工业区域。 施工地面要求 (一) 水泥、水磨石地面必须平整、坚硬、不得有松动裂缝或脱落现象。 (二) 新施工的水泥地面需经过20-25天的充分干燥,经测试含水率不超过8%时方能施工。 (三) 一楼地面、地下室需施工防潮层。 (四) 0℃以下不能施工。
Apply the scope The electronics assembles the car a car a light industry district. Construction ground request (One) the cement, Water millstone ground must be neat, strong and tough, cannot loosen to move the crack or shed off the phenomenon. (two)the cement ground of the new construction needs through 20-25 days well dry, Was contained by test the rate of water not then can start construction over the hour of 8% (three)the first floor ground, ground floor needs the construction defends the tide layer.
Product characteristic Bear the impact, bear the heavy pressure, bear the eclipse, not peeling off, the anti-is cracked and does not rise .The function of the whole is good, bearing the difference inure change, for insulate the material.
|